AWS A5.5 E8016-B8 Uila Electrodes Low Alloy Uila Uila Uila La'au Arc Uila Mea

Fa'amatalaga Puupuu:

E8016-B8 Uila Electrodes: Uilaina o 9% Cr-1% Mo uamea ma 9% Cr - 2% Mo uamea faʻaaogaina mo le eletise ma le vaʻa maualuga.


Fa'amatalaga Oloa

Faailoga o oloa

TALOSAGA:

Uilaina o uʻamea 9% Cr-1% Mo ma 9% Cr - 2% Mo uamea faʻaaogaina mo le eletise ma le vaʻa maualuga.

FAAMATALAGA:

PA-8016-B8 o se eletise hydrogen maualalo e uʻamea uʻamea e aofia ai 9%Cr-1% Mo.Ua mamanuina mo u'amea vevela maualuga ma u'amea mo auaunaga o le hydrogen vevela, aemaise lava i pisinisi petrochemical.E mafai ona faʻamaonia le eletise mo lona malosi maualuga, malosi lelei ma le vevela tele.

FAAMATALAGA I LE FA'A'UGA:

1. Fa'amamago eletise i le 350-400 ° C mo le tusa ma le tasi le itula a'o le'i fa'aoga ma teu le eletise i le 100-150 ° C pe a uma ona fa'agogo ma le fa'alogo lelei e aloese mai le susu.

2. Fa'aaoga auala la'asaga i tua po'o taia le arc i luga o se tama'i ipu u'amea ua saunia mo lea fa'amoemoe fa'apitoa e puipuia ai le fa'aulu i le arc amata.

3. Ia faapuupuu le arc e mafai ai.

4. Fa'avevela ile 100-150°C.O le vevela e faʻaaogaina e eseese e tusa ai ma le mafiafia o le ipu ma le ituaiga uamea e faʻafefe.

5. Fa'alogo lelei ia 'aua ne'i sili atu i totonu o le vevela talafeagai ona o le tele o le vevela e mafua ai le fa'aleagaina o tau o le a'afiaga ma maua ai le malosi o le u'amea.

IV.FA'AVAE FA'AVAE FA'AVAE O LE FA'ASAUINA (%):

C

Si

Mn

Cr

Mo

0.06

0.42

0.68

9.38

1.05

V. TULAGA FA'AVAE FA'AVAE FA'AVAE O LE UA'AU UIGA:

Malosi Tetele N/mm2(Ksi)

Fa'ailoga N/mm2

(Ksi)

Fa'aumi %

PWHT

705 (102)

560 (81)

24

740°C x 1 itula

VI.TULAGA UIGA: TULAGA UMA

VII.TELE MA LE VAEGA FAATUATUA NEI (AC/DC+):

Diamita (mm)

2.5

3.2

4.0

5.0

Umi (mm)

350

350

400

400

Apere

Mafolafola

55 - 85

90 - 130

130 - 180

180 - 240

V & OH

50 - 80

80 - 115

110 - 170

150 - 200