La'au Uila AWS A5.11 ENiCrFe-3 La'au Uila Fa'aigoa Nikeli, La'au Uila Uila

Fa'amatalaga Puupuu:

Ni307-3 (AWS ENiCrFe-3) o se eletise faʻavae nickel faʻatasi ai ma le paʻu sodium maualalo-hydrogen.Fa'aaogā le DCEP (fa'atonu eletise eletise i le taimi nei).


Fa'amatalaga Oloa

Faailoga o oloa

Nikeli ma le nikeli u'umea fa'aeletise

Ni307-3                                                     

GB/T ENi6182

AWS A5.11 ENiCrFe-3

Faʻamatalaga: Ni307-3 o senikeli-fa'avae eletise fa'atasi ma le fa'apalapala sodium maualalo-hydrogen.Fa'aaogā le DCEP (fa'atonu eletise eletise i le taimi nei).E lelei le tete'e ona o le uelo o lo'o i ai se aofa'i o manganese, niobium, ma isi elemene fa'afefiloi.

Fa'aoga: E fa'aaogaina mo le ueloina onikeli-chromium-u'amea u'amea (e pei o le UNS N06600) ma le fa'afefeteina o le sila.O le vevela galue e masani lava e le maualuga atu i le 480 ° C, ma e lelei le teteʻe o le ta.Talafeagai mo atomic ogaumu oomi vaa ma tane vailaau uelo.

 

Su'ega vaila'au o u'amea u'amea(%):

C

Mn

Fe

P

S

Si

Cu

≤0.10

5.0 ~ 10.0

≤10.0

≤0.020

≤0.015

≤1.0

≤0.5

Ni

Ti

Mo

Nb

Ta

Isi

 

≥60.0

≤1.0

13.0 ~ 17.0

1.0 ~ 3.5

≤0.30

≤0.50

 

 

Tulaga fa'ainisinia o u'amea u'amea:

Su'ega mea

Malosi fa'asa

Mpa

Tuuina atu le malosi

Mpa

Fa'aumiumi

%

Fa'amaonia

≥550

≥360

≥27

 

Fautuaina le taimi nei:

u'amea lautele

(mm)

2.5

3.2

4.0

5.0

Uu fa'asolo

(A)

60 ~ 90

80 ~ 100

110 ~ 150

130 ~ 180

 

Fa'aaliga:

1. E tatau ona tao le eletise mo le 1 itula i le 300 ℃ aʻo leʻi faʻaogaina le faʻaogaina;

2. E taua tele le fa'amamāina o le ea, suau'u, vai, ma mea leaga i luga o vaega uelo a'o le'i uelo.Taumafai e fa'aoga se arc pupuu e uelo ai.

 