Uila u'amea Uila maualalo Electrode J506NiMA, J507NiMA GB/T E5016-G E5015-G AWS E7018-G E7015-G

Fa'amatalaga Puupuu:

J506NiMA (AWS E7018-G) ma J507NiMA (AWS E7015-G) o susū-absorbing ultra-maualalo hydrogen-coated maualalo-alloy uamea electrodes.


Fa'amatalaga Oloa

Faailoga o oloa

Uila Uila Uila maualalo Electrode

J506NiMA, J507NiMA                                                     

GB/T E5016-G E5015-G

AWS E7018-G E7015-G

Fa'amatalaga: O le J506NiMA ma le J507NiMA o le susū-susua e sili atu le maualalo o le hydrogen-coated low-alloy steel electrodes.O le u'amea teuina e sili ona lelei le palasitika, maualalo le vevela ma le ta'e tete'e, ma e mafai ona uelo i tulaga uma.O le faʻapipiʻi e faʻasaʻo i le faʻafefe o le susu.A maeʻa ona tao le electrode i le 400 ° C x 1h ma paka i totonu o se siʻosiʻomaga ma le susu faʻatusatusa ≥ 80% mo le 4 itula, o loʻo faʻamalieina e le susu o le faʻapipiʻi mea e manaʻomia mo le faʻaaogaina.

Talosaga: E faʻaaogaina mo le faʻapipiʻiina o suauʻu suauu, vaʻa, vaʻa mamafa, ma isi fausaga e faia iuamea kaponi ma uamea uamea maualalo.

 

Su'ega vaila'au o u'amea u'amea(%):

C

Mn

Si

Ni

S

P

Fa'amaonia

≤0.12

≥1.00

≤0.50

≤0.60

≤0.035

≤0.040

 

Tulaga fa'ainisinia o u'amea u'amea:

Su'ega mea

Malosi fa'asa

Mpa

Tuuina atu le malosi

Mpa

Fa'aumiumi

%

Tau a'afiaga (J)

-46℃

Fa'amaonia

≥490

≥390

≥22

≥27

 

Fa'asalalauina o mea o lo'o i totonu ole u'amea o lo'o teuina: ≤5.0mL/100g (chromatography kesi po'o metotia mercury)

Susū i totonu o paluga eletise: ≤0.30%

Asiasiga X-ray: Ou te togi

 

Fautuaina le taimi nei:

u'amea lautele

2.5

3.2

4.0

5.0

Uelo Uila

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Fa'aaliga:

1. E tatau ona tao le electrode mo le 1 itula i le 350 ~ 400 ℃ aʻo leʻi faʻaogaina le faʻaogaina;

2. E taua tele le fa'amamāina o le ea, fua o le suau'u, vai, ma mea leaga i luga o vaega uelo a'o le'i u'uina;

3. Fa'aaoga le fa'agaioiga pu'upu'u pe a uelo.O le ala uelo vaapiapi e talafeagai.

 