AWS ERNiCrMo-7 Nickel Alloy Uili Uili Mig ma Tig Uaea, Arc Uili Uila Fa'atau Uila Sili.

Fa'amatalaga Puupuu:

ERNiCrMo-10 o loʻo faʻaaogaina mo le faʻaogaina o mea faʻavae nickel-chromium-molybdenum ia i latou lava, uʻamea ma isi mea faʻavae nickel, ma mo uʻamea faʻapipiʻi.E mafai ona fa'aogaina e u'amea ai le lua, u'amea u'amea super duplex.


Fa'amatalaga Oloa

Faailoga o oloa

FA'AMATALAGA O O'OGA:

AWS: A5.14

E tusa ai ma Fa'ailoga: AWS A5.14 ASME SFA A5.14

Fa'agasologa o le Uelo: GMAW & ASAW Fa'asologa Fa'asologa

ERNiCrMo-10 o loʻo faʻaaogaina mo le faʻaogaina o mea faʻavae nickel-chromium-molybdenum ia i latou lava, uʻamea ma isi mea faʻavae nickel, ma mo uʻamea faʻapipiʻi.E mafai ona fa'aogaina e u'amea ai le lua, u'amea u'amea super duplex.

AWS Chemical Composition Manaoga

C = 0.015 maualuga Cu = 0.50 maualuga
Mn = 1.0 maualuga Ni = Toe
Fe = 3.0 maualuga Co = 2.0 maualuga
P = 0.04 maualuga Cr = 14.0 - 18.0
S = 0.03 maualuga Mo = 14.0 - 18.0
Si = 0.08 maualuga W = 0.50 maualuga
Isi = 0.50 maualuga Ti = 0.70 maualuga

Fa'amolemole vili mo nisi fa'amatalaga ma tele o lo'o avanoa:

Fa'atatauga

ERNiCrMo-7 o loʻo faʻaaogaina mo le faʻapipiʻiina o mea faʻavae nickel-chromium-molybdenum ia te ia lava, uʻamea ma isi mea faʻavae nickel ma mo le faʻapipiʻiina o uamea i mea faʻapipiʻi NI-CR-MO.

FAIGA FA'AVAE:

Tulaga Kemisi % (Masa masani)
C = 0.01 Cr = 16.5 Ni = Paleni
Fe = 2.20 Mo = 15.75
Teuina uma Meatotino Uila % (AW)
Malosi Tetele 113,00 psi
Fa'aumiumi 29%

TUUINA O LE CHARPY-V-NOTCH A'afiaga o mea totino:

E le agavaa ai

Fua Fautuaina Uila mo MIG ma SAW Uila o nikeli Alloys
Fa'agasologa Tatami ole Uaea Malosi (V) Amperage (A) kesi
MIG .035 inisi 26 - 29 150 - 190 75 % Argon + 25% Helium
.045 inisi 28 - 32 180 - 220 75 % Argon + 25% Helium
1/16 inisi 29 - 33 200 - 250 75 % Argon + 25% Helium
SA 3/32 inisi 28 - 30 270 - 350 E mafai ona fa'aaogaina Flux talafeagai.
1/8 inisi 29 - 32 350 - 450 E mafai ona fa'aaogaina Flux talafeagai.
5/32 inisi 30 - 33 400 - 550 E mafai ona fa'aaogaina Flux talafeagai.