AWS ER5183 Aluminum Uili Uila Alumini MIG uelo Uila Tig Uaea

Fa'amatalaga Puupuu:

ER5183 e talafeagai mo le MIG uʻumea le alumini magnesium alumini e manaʻomia le malosi maualuga ma afai o le uʻamea faavae o le 5083 poʻo le 5654 o le a sili atu le maualuga o le malosi.E faʻaaogaina lautele mo le faʻapipiʻiina o fausaga alumini alumini magnesium o vaʻa, faʻasalalauga i fafo, locomotives & taʻavale, taavale afi, pusa, vaʻa cryogenic ma isi.


Fa'amatalaga Oloa

Faailoga o oloa

ER5183 e talafeagai mo le MIG uʻumea le alumini magnesium alumini e manaʻomia le malosi maualuga ma afai o le uʻamea faavae o le 5083 poʻo le 5654 o le a sili atu le maualuga o le malosi.E faʻaaogaina lautele mo le faʻapipiʻiina o fausaga alumini alumini magnesium o vaʻa, faʻasalalauga i fafo, locomotives & taʻavale, taavale afi, pusa, vaʻa cryogenic ma isi.O lona u'amea u'amea e lelei le tete'e atu i brine corrosion.

Tulaga uelo: F, HF, V

Ituaiga o le taimi nei: DCEP

FAAMATALAGA:

Taofi lelei le afifi o le uaea a'o le'i uelo.

O mea uma e lua e faʻapipiʻiina o le uelo ma le uaea e tatau ona faʻamama ese mea leaga o le faʻaleagaina o le suauʻu, faʻafefe o le oxide, susu ma isi.

Ina ia maua foliga lelei o le uelo e tatau ona muai faamafanafanaina le u'amea faavae i le 100 ℃-200 ℃ aʻo leʻi uelo pe afai o lona mafiafia e 10mm pe sili atu.

E sili atu le tuʻuina o se subplate i lalo o le sone uelo e faʻapipiʻi ai le uʻamea liusua ina ia mautinoa le faʻaogaina atoatoa o le uelo.

E tusa ai ma tulaga uelo ma le mafiafia o le uamea faavae eseese kasa talita e tatau ona filifilia, e pei o le 100% Ar, 75% Ar + 25% He, 50% Ar + 50% He, ma isi.

O tulaga uelo o loʻo taʻua i luga mo naʻo le faʻamatalaga ma e sili atu le faia o se faʻataʻitaʻiga faʻataʻitaʻiga e tusa ai ma le poloketi aʻo leʻi tuʻuina i totonu o le uelo aloaia.

ER5183 FA'AVAE FA'AVAE O METAL TU'U (%):

SI FE CU MN MG CR ZN TI AI BE
Tulaga ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Paleni ≤0.0003
masani 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Paleni 0.0001

FA'AIGA MESINI O METAL TU'U (AW):

MALOSI TELE RM (MPA) LE MALOSI O LE FA'ATA'IGA (MPA) ELONGATION A4 (%)
masani 280 150 18

Tele & Fautuaina i le taimi nei mo MIG (DC+):

UIGA UILI LE TAMETER (MM) 1.2 1.6 2.0
U'u Uila (A) 180-300 200-400 240-450
Uila Volta (V) 18-28 20-20 22-34

TETEA & FAATUATUA I LE TAIMI MO TIG (DC¯):

UIGA UILI LE TAMETER (MM) 1.6-2.5 2.5-4.0 4.0-5.0
U'u Uila (A) 150-250 200-320 220-400

  • Muamua:
  • Sosoo ai: