AWS E7015 Uila Uila

Fa'amatalaga Puupuu:

AWS A5.1 E7015 o le maualalo-hydrogen sodium coated carbon sila electrode.


Fa'amatalaga Oloa

Faailoga o oloa

AWS A5.1 E7015 o le maualalo-hydrogen sodium coated carbon sila electrode.

E7015 u'i eletise e tatau ona faagaoioia i DCEP.E lelei tele le fa'aogaina o le uelo lea e mafai ai ona fa'atino uma-tulaga uelo, e mautu arc, aveese le slag e faigofie ma e maualalo le spatter.O le u'amea teuina e lelei le fa'atinoina o masini ma ta'eta'ei-tetee, lea e ofoina lelei le maualalo vevela faigata.

Fa'atatauga

AWS A5.1 E7015 o loʻo faʻaaogaina i le faʻaogaina o le uʻamea-carbon uʻamea ma le maualalo o fausaga e pei o le 16Mn, 09Mn2Si, 09Mn2V ma le uamea faʻaaogaina i le fausiaina o vaa e pei o A, B, D, E. E faʻaaogaina foi i papatusi mafiafia ma o fausaga uamea kaponi e faigata ona uelo.

E tusa ai ma tulaga masani

GB/T 5117 E5015

AWS A5.1 E7015

ISO 2560-BE 49 15 A

Faamoemoega: AWS A5.1 E7015 o loʻo faʻaaogaina i le faʻaogaina o le uʻamea-carbon uʻamea ma le maualalo-faʻapipiʻi fausaga e pei o 16Mn, 09Mn2Si, 09Mn2V ma uamea faʻaaogaina i le faufale e pei o A, B, D, E. E faʻaaogaina foi i le sila mafiafia. papatusi ma fausaga uamea carbon e faigata ona uelo.

Tulaga Fa'aisi (%)

Fa'asu'esu'ega o vaila'au

C

Mn

Si

S

P

Ni

Cr

Mo

V

Tau Fa'amautinoa

≤

0.15

≤

1.60

≤

0.90

≤0.035

≤0.035

≤

0.30

≤

0.20

≤

0.30

≤

0.08

I'uga Lautele

0.082

1.10

0.58

0.012

0.021

0.011

0.028

0.007

0.016

Meatotino Fa'ainisinia o Uamea ua teuina(Kesi Puipuia:CO2)

Mea Su'ega

Rm(MPa)

ReL(MPa)

A(%)

KV2(J)

-20℃ -30℃

Tau Fa'amautinoa

≥490

≥400

≥20

≥47

≥27

I'uga Lautele

550

450

32

150

142

X-Ray Leitio-kalafi Manaoga Su'ega: Vasega I

Fa'asino i le taimi nei(DC+)

Diamita(mm)

Φ2.5

Φ3.2

Φ4.0

Φ5.0

Amperage(A)

60~100

80~140

110~210

160~230

Fa'amatalaga:

1. E tatau ona muaʻi faʻamafanafanaina le eletise i le vevela o le 350 ° C mo le 1 itula.Fa'avela le tootoo i so'o se taimi e fa'aaoga ai.

2. O mea leaga e pei o le 'ele, stains suau'u ma le susu e tatau ona aveese mai le mea faigaluega.

3. O le arc puupuu e manaʻomia e faʻatino ai le uelo.E sili le ala uelo vaapiapi.


  • Muamua: