W707Ni La'au Uila La'au Fa'atau Uila Maualalo Electrode La'au Uila Maulalo

Fa'amatalaga Puupuu:

W707Ni o se electrode uʻamea maualalo-vevela o loʻo i ai Ni i se faʻapipiʻi sodium maualalo-hydrogen.


Fa'amatalaga Oloa

Faailoga o oloa

Uamea Maualalo MaualaloUeloElectrode

W707Ni                                                     

GB/T E5515-C1

Faʻamatalaga: W707Ni o se eletise uʻamea maualalo maualalo o loʻo i ai le Ni i totonu o se faʻamalo maualalo o le sodium.Fa'aaoga le DCEP (fa'atonu eletise eletise) ma e mafai ona uelo i tulaga uma.O le u'amea na teuina o lo'o i ai pea le malosi o a'afiaga ile -70°C.

Fa'aoga: Fa'aaogaina mo le ueloina o le sila maualalo vevela pei ole 2.5Ni.

 

Su'ega vaila'au o u'amea u'amea(%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

≤0.60

2.00 ~ 2.75

≤0.020

≤0.025

 

Tulaga fa'ainisinia o u'amea u'amea:

Su'ega mea

Malosi fa'asa

Mpa

Tuuina atu le malosi

Mpa

Fa'aumiumi

%

Tau a'afiaga (J)

-70℃

Fa'amaonia

≥540

≥440

≥17

≥27

 

Fa'asalalauina o le hydrogen i totonu o u'amea ua teuina: ≤6.0mL/100g (metotia glycerin) po'o le ≤10mL/100g (mecury po'o le gas chromatography method)

Asiasiga X-ray: Ou te togi

 

Fautuaina le taimi nei:

(mm)

u'amea lautele

2.0

2.5

3.2

4.0

5.0

(A)

Uelo Uila

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 Fa'aaliga:

  1. E tatau ona tao le eletise mo le 1 itula i le 350 ℃ aʻo leʻi faʻaogaina le faʻaogaina;
  2. E taua tele le fa'amamāina o le ele, fua o le suau'u, vai, ma mea leaga i luga o vaega uelo a'o le'i uelo;
  3. Taumafai e fa'aoga le malosi o le laina la'ititi pe a uelo, fa'apipi'i fa'atele ma fa'asolo fa'atasi.

 