Uaea Fa'apipi'i Malosi ER410NiMo

Fa'amatalaga Pupuu:

O le ER410NiMo o se uaea mafiafia uamea e le gaoia e fai i le martensitic ma e iai le tuufaatasiga o vailaʻau e aofia ai le 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, ma le 0.40 – 0.70% Mo.

Fa'amatalaga o le oloa

Fa'ailoga o Oloa

Tulaga Fa'atonuina

-NB/T 47018.3-2017 S410NiMo
-GB/T 29713-2013 S410NiMo
-AWS A5.9M-2022 ER410NiMo
-ASME SFA-5.9M-2023 ER410NiMo
-YB/T 5092-2016 H05Cr12Ni4Mo
Meafaitino Tutusa: 1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM

Fa'amatalaga

O le ER410NiMo o se uaea malosi uamea e le gaoia ma e iai le tuufaatasiga o vailaʻau e aofia ai le 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, ma le 0.40 – 0.70% Mo. E talafeagai mo le faʻapipiʻiina o le kesi (e pei o le TIG/MIG) i tulaga uma. I le taimi o le faʻapipiʻiina, e mautu le arc, ma o le uʻamea ua faʻapipiʻiina e iai le teteʻe lelei i le cavitation, teteʻe i le oneone,
ma meatotino fa'amekanika. E masani lava e le mana'omia le fa'avevela muamua a'o le'i fa'apipi'iina; o le togafitiga fa'avevela pe a uma ona fa'apipi'iina (PWHT) i le 580~620℃ mo le 2 itula (soso'o ai ma le fa'amālūlūina o le ea, AC) e fautuaina e tusa ai ma mana'oga o le fa'aoga. O le u'amea ua fa'apipi'iina e mafai ona fa'amekanika ma talafeagai mo masini fa'amalosi.

Talosaga

Ua mamanuina mo le fa'avevela o le u'amea ASTM CA6NM, u'amea e le gaoia 410/410S/405, ma u'amea fa'apena e 13%Cr – 4%Ni. O fa'aoga masani e aofia ai masini e fa'amamafa ai le mamafa (e ogatasi ma tulaga fa'atonuina o va'a e fa'amamafa ai le mamafa), lau o turbine, valve, paipa e maualuga le mamafa, ma vaega fa'atulagaina e mana'omia ai le tete'e atu i le 'ele ma le ofuina.

Fa'atulagaga Fa'akemikolo o le U'amea Fa'apipi'i (%)

Elemene C Cr Ni Mo Mn Si P S Cu
Manaoga ≤0.06 11.0-12.5 4.0-5.0 0.40-0.70 ≤1.00 ≤0.60 ≤0.050 ≤0.020 ≤0.75
I'uga o le Su'ega 0.011 12.21 4.70 0.54 0.58 0.47 0.016 0.008 0.01

 

Uiga Fa'amekanika o Uamea ua Fa'aputuina

Igoa o le Su'ega Malosiaga o le Tete'e (MPa) Fa'aloloa% X-Ray Su'ega o le A'afiaga (+20 ℃)J Ma'a'a HB
Manaoga ≥760 ≥15 Vasega I – –
I'uga o le Su'ega 830 18 Vasega I 65 250-310

Fa'atulagaga Fa'aleleia o le Uelo

Kasa Puipuia: Argon(Ar) po'o Ar+1-2% O2 (mo le uelo TIG/MIG, fetu'una'i e tusa ai ma faiga fa'apitoa).

 

Faasilasilaga

1. Ia mautinoa o le uaea e mama ma sa'oloto mai le suau'u, ele, po'o le susu a'o le'i fa'aaogaina ina ia 'alofia ai le a'afia ai o le lelei o le uelo.

2. Tausia le mama o le kasa ma le sa'o o le tafe e puipuia ai le porosity ma le māvaevae e mafua mai i le hydrogen.