Fa'amatalaga Pupuu:

Mo le fa'avevela o le arc alumini ua fa'afefiloi ma le kopa, silicon, ma le magnesium


Fa'amatalaga o le oloa

Fa'ailoga o Oloa

EN 573-3: E AlSi12

DIN 1732: EL-Al Si12

VAEGA & FA'AOGA:

Mo le fa'avevela o le arc, e fa'aaoga ai le alumini ua fa'afefiloi ma le kopa, silicon, ma le magnesium.

E sili fo'i mo le fa'apipi'iina o ituaiga alumini eseese.

Eleketo uelo alumini 12% Silicon fa'atasi ai ma le u'amea e si'itia e ia lava. O isi vasega alumini e pei o le Al 99, Al Mn, ma isi.

Ota e si'i e ia lava i se tulaga tulaga ese.

E umi se taimi e teu ai le vali pa'epa'e mama e sili atu lona tete'e atu i le susu nai lo oloa masani.
E mafai ona gaosia i le tele o lanu eseese e te manaʻo ai.

E maua i totonu o apa mama toso PURE ALUMINUM ua fa'amaufa'ailogaina lelei pe i totonu o taga pepa alumini ua fa'apipi'i i le vacuum mo se taimi umi e teu ai.

O loʻo maua foʻi i le tulaga TIG o se numera aitema 6047, i le tulaga MIG o se numera aitema 7091 ma o se laina e leai se paʻu.

O LE TORCH BRAZING ALLOY E PEI O LE KODE O LE AItema 2191:

Su'esu'ega Uma o U'amea Fa'apipi'i (Mamafa Masani%)
Lanu Flux: Lanu Pa'epa'e po'o Lanu Fa'apitoa
12.1 .001 .15 .01 .003 .001
Si Cu Fe Mg Mn Zn
Tafe o le Uelo ma Fa'atonuga
Taimi Fautuaina: DC Fa'afeagai (+)
Lapoa (mm) 3/32 (2.5) 1/8 (3.25)
Amperage Maualalo 50 70
Amperage Maualuga 80 120

Tomai Fa'apipi'i: Amata i le fa'aaogaina o le vaega pito i luga o le laina amperage. Fafaga vave le eletise ma gaoioi vave ma tausia se va e matua vavalalata lava.
Tulaga Fa'apipi'i: Mafolafola, Fa'alava

FUA FA'ATAU O LE TEUINA:

Lapoa (mm) Umi (mm) U'amea fa'a'u'u/Elektroda Electrodes i le pauna (kg) o le Weldmetal Taimi o le Fa'aputuga o le Mea Min/lb (kg) Fa'atulagaga o le Amperage Fuainumera o le Toe Fa'aleleia
3/32 (2.5) 14″(350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

FUA MA LE AFIFAGA FA'ATATAU O LE ELECTRODE:

3/32 (2.5) 1/8 (3.25)
Umi (mm) 14″ (350) 14″ (350)
Eletise / pauna 49 33
Eletise / kg 108 73

  • Muamua: