Fa'amatalaga Puupuu:

O le A002 (AWS E308L-16) o se eletise uʻamea uʻamea Cr19Ni10 ultra-maualalo ma le titanium-calcium coating.


Fa'amatalaga Oloa

Faailoga o oloa

Electrode Uila Uila

A002                                                 

GB/T E308L-16

AWS E308L-16

Fa'amatalaga: A002 o se eletise u'amea u'amea sili ona maualalo le carbon Cr19Ni10 fa'atasi ma le titanium-calcium coating.E mafai ona faʻaaogaina mo le AC ma le DC faʻatasi ai ma le lelei o le faʻatinoga.O le carbon anotusi o le uamea teuina o ≤0.04% lea e maua ai le lelei anti-intergranular corrosion faatinoga.

Talosaga: E faʻaaogaina mo le faʻapipiʻiina o fausaga uʻamea uʻamea ultra-low carbon Cr19Ni10, ma e mafai foi ona faʻaaogaina mo 06Cr18Ni1Ti faʻamaʻi faʻamaʻi faʻamaʻi uʻamea fausaga uʻamea o loʻo maualalo le vevela galue nai lo le 300 ° C;e masani ona faʻaaogaina mo le gaosiga o filo faʻapipiʻi, vailaʻau vailaʻau, suauu ma isi meafaigaluega.

 

Su'ega vaila'au o u'amea u'amea(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

9.0 ~ 11.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Tulaga fa'ainisinia o u'amea u'amea:

Su'ega mea

Malosi fa'asa

Mpa

Fa'aumiumi

%

Fa'amaonia

≥520

≥35

 

Fautuaina le taimi nei:

u'amea lautele

(mm)

2.0

2.5

3.2

4.0

5.0

Uelo Uila

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Fa'aaliga:

1. E tatau ona tao le eletise mo le 1 itula i le 150 ℃ aʻo leʻi faʻaogaina le faʻaogaina;

2. Fa'aaoga le mana DC i le tele e mafai ai, ma o le taimi nei e le tatau ona tele tele e aloese ai mai le mumu o le tootoo uelo;

3. O le puipuiga o le corrosion ma le ferrite o loʻo i totonu o le uʻamea teuina e fuafua i le maliliega faʻalua o le tuʻuina atu ma le manaʻoga.

 

Wenzhou Tianyu Electronic Co., Ltd. na faʻatūina i le 2000. Ua matou galulue i le gaosiga o le uʻamea eletise, uʻamea uʻamea, ma le faʻaaogaina o meaʻai mo le silia ma le 20 tausaga.

O a tatou oloa autu e aofia ai eletise u'amea u'amea, uaea u'amea uamea kaponi, uaea u'amea u'amea maualalo, fa'aeletise u'amea fa'afefete, u'amea u'amea nickel & cobalt, uaea u'amea mālūlū & uaea u'amea maualalo, uaea u'amea uamea, uaea fa'a'au'au fa'alu, uaea uaea fa'afefeteina. uaea u'amea alumini, uelo fa'aluulu.uaea, nickel & cobalt u'umea uaea, apamemea u'amea uaea, TIG & MIG uaea, tungsten electrodes, carbon gouging electrodes, ma isi mea uelo & consumables.