AWS ENi-C1 (Z308) u'amea mama u'amea u'amea electrode nikeli 99 u'amea u'amea Arc Stick Electrodes Ni99

Fa'amatalaga Puupuu:

AWS ENi-C1 (Z308) o se uʻamea uʻamea electrode ma se uʻamea uʻamea maualalo autu ma se faʻapipiʻi malosi graphitized.


Fa'amatalaga Oloa

Faailoga o oloa

U'amea U'amea Electrode

Z308                                                     

GB/T EZNi-1

AWS A5.15 ENi-C1

Fa'amatalaga: Z208 o se u'amea u'amea electrode ma le maualalo carbon sila autu ma se malosi graphitized coating.E mafai ona faʻaaogaina mo AC ma DC.E mafai ona fa'aefuefu le u'amea pe a fa'amalie lemu, ae leaga lona tete'e.

Fa'aaogāga: Fa'aaogā e toe fa'aleleia ai fa'aletonu i u'amea efuefu.

 

Su'ega vaila'au o u'amea u'amea(%):

C

Si

Mn

S

Ni

Fe

O isi

≤2.0

≤2.5

≤1.0

≤0.03

≥90

≤8.0

≤1.0

 

Fautuaina le taimi nei:

u'amea lautele

(mm)

2.5

3.2

4.0

Uu fa'asolo

(A)

65 ~ 90

90 ~ 110

120 ~ 150

 

Fa'aaliga:

1. E tatau ona tao le electrode mo le 1 itula i le 150 ℃ aʻo leʻi faʻaogaina le faʻaogaina;

2. E mafai ona faʻaumatia le faʻalavelave i totonu o le faʻaleleia o le uelo e ala i le sasaina o le uelo e aloese ai mai taʻe.

 

 

Wenzhou Tianyu Electronic Co., Ltd. na faʻatūina i le 2000. Ua matou galulue i le gaosiga o le uʻamea eletise, uʻamea uʻamea, ma le faʻaaogaina o meaʻai mo le silia ma le 20 tausaga.

O a tatou oloa autu e aofia ai eletise u'amea u'amea, uaea u'amea uamea kaponi, uaea u'amea u'amea maualalo, fa'aeletise u'amea fa'afefete, u'amea u'amea nickel & cobalt, uaea u'amea mālūlū & uaea u'amea maualalo, uaea u'amea uamea, uaea fa'a'au'au fa'alu, uaea uaea fa'afefeteina. uaea u'amea alumini, uelo fa'aluulu.uaea, nickel & cobalt u'umea uaea, apamemea u'amea uaea, TIG & MIG uaea, tungsten electrodes, carbon gouging electrodes, ma isi mea uelo & consumables.

 