AWS E9016-B3 Electrode u'amea u'amea e tete'e vevela R406 u'amea u'amea etetee

Fa'amatalaga Puupuu:

R406 (AWS E9016-B3) o se pearlitic vevela-tetesua uʻamea electrode ma le maualalo-hydrogen palasitika coating o loo i ai 2.5% Cr - 1% Mo.


Fa'amatalaga Oloa

Faailoga o oloa

Molybdenum ma Chromium Molybdenum Tete'e vevelaUili uameaElectrode

R406                                                     

GB/T E6016-B3

AWS A5.5 E9016-B3

Faʻamatalaga: R406 o se pearlitic vevela-tetesua uamea electrode ma le maualalo-hydrogen palasitika coating o loo i ai 2.5% Cr - 1% Mo.Both AC ma DC e mafai ona faaaogaina, ma e mafai ona uelo i tulaga uma.O le uelo e tatau ona muaʻi faʻamafanafanaina i le 160 ~ 200 ° C aʻo leʻi faʻapipiʻiina.

Talosaga: Faʻaaogaina mo le faʻapipiʻiina o le uʻamea Cr2.5Mo pearlitic vevela faʻafefeteina fausaga uʻamea, e pei o paipa maualuga-vevela ma maualuga-omiga ma le vevela o loʻo galue i lalo ole 550 ° C, masini vailaʻau faʻapipiʻi, ma mea faʻapipiʻi suauu.

 

Su'ega vaila'au o u'amea u'amea(%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

2.00 ~ 2.50

0.90 ~ 1.20

≤0.030

≤0.030

 

Tulaga fa'ainisinia o u'amea u'amea:

Su'ega mea

Malosi fa'asa

Mpa

Tuuina atu le malosi

Mpa

Fa'aumiumi

%

Tau a'afiaga (J)

Temp masani.

Fa'amaonia

≥590

≥490

≥15

≥47

 

Fa'asalalauina o le hydrogen i totonu o le uamea ua teuina: ≤4.0mL/100g (auala glycerin)

 

Asiasiga X-ray: Ou te togi

 

Fautuaina le taimi nei:

u'amea lautele

(mm)

2.5

3.2

4.0

5.0

UeloI le taimi nei

(A)

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Fa'aaliga:

1. E tatau ona tao le eletise mo le 1 itula ile 350 ℃ aʻo leʻi faʻaogaina le faʻaogaina;

2. E taua tele le fa'amamāina o le ele, fua o le suau'u, vai, ma mea leaga i luga o vaega uelo a'o le'i uelo.

 