AWS A5.11 ENiCrFe-2 Nickel Based Welding Electrode Ni307-2 Low Hydrogen Nickel Welding Rod Arc Welding, Tyue Brand Welding Stick

Fa'amatalaga Pupuu:

O le Ni307-2 (AWS ENiCrFe-2) o se eletise e fa'avae i le nickel ma e ufiufi i le sodium maualalo le hydrogen. Fa'aaoga le DCEP (direct current electrode positive).


Fa'amatalaga o le oloa

Fa'ailoga o Oloa

Electrode Fa'amauina o le Nickel ma le Nickel Alloy

Ni307-2                                                     

GB/T ENi6133

AWS A5.11ENiCrFe-2

Fa'amatalaga: O le Ni307-2 o se eletise e fa'avae i le nickel ma e ufiufi i le sodium maualalo le hydrogen. Fa'aaoga le DCEP (electrode current direct). Talu ai o lo'o iai i le uelo se aofa'i patino o le molybdenum, niobium ma isi elemene fa'afefiloi, o le u'amea ua fa'aputuina e iai le tete'e lelei i le māvaevae.

 

Fa'aoga: Fa'aaogaina mo le fa'avevela o le nickel-chromium-iron alloys (e pei o le UNS N08800, UNS N06600), e talafeagai faapitoa mo le fa'avevela o u'amea eseese, fa'avevela o le vaega fesuia'i ma le fa'avevela o luga, ma e mafai foi ona fa'aaogaina pe a o'o atu le vevela o le galuega i le 980 ° C, ae e mafai ona tete'e atu i le fa'ama'i pe a maualuga atu le vevela i le 820 ° C. Fa'aitiitia le malosi ma le malosi.

 

Fa'asologa fa'akemikolo o le u'amea fa'apipi'i (%):

C

Mn

Fe

Si

Cu

Ni

≤0.10

1.0 ~ 3.5

≤12.0

≤0.8

≤0.5

≥62.0

Cr

Nb + Ta

Mo

S

P

Isi

13.0 ~ 17.0

0.5 ~ 3.0

0.5 ~ 2.5

≤0.015

≤0.020

≤0.50

 

Uiga fa'amekanika o le u'amea fa'apipi'i:

Mea fa'ata'ita'i

Malosiaga o le tensile

Mpa

Malosiaga o le fua

Mpa

Fa'aloloa

%

Fa'amaonia

≥550

≥360

≥27

 

Taimi nei fautuaina:

Lapo'a o le tootoo

(mm)

2.5

3.2

4.0

5.0

Tafe o le uelo

(A)

60 ~ 90

80 ~ 100

110 ~ 150

130 ~ 180

 

Fa'aaliga:

1. E tatau ona tao le eletise mo le 1 itula i le vevela e tusa ma le 300 ℃ a'o le'i fa'agaoioia le uelo;

2. E taua tele le fa'amamāina o le 'ele, suāu'u, vai, ma mea leaga i vaega o le uelo a'o le'i ueloina. Taumafai e fa'aaoga se 'arc' pu'upu'u e uelo ai.

 