ZELLER D350(UTP DUR 350) ELECTRODE TETEE I LE OFU

Fa'amatalaga Pupuu:

E matuā fetaui lelei le UTP DUR 350 mo vaega e tete'e atu i le ofuina i le u'amea MnCrV.

Fa'amatalaga o le oloa

Fa'ailoga o Oloa

Fa'avasegaga
DIN 8555/EN 14700
E1-UM-350/E Fe1
Uiga ma le fanua o le faʻaaogaina
E matuā fetaui lelei lava le UTP DUR 350 mo vaega e tete'e atu i le ofuina i luga o vaega ua fa'apipi'iina i le MnCrV, e pei o
rana, uili ala, uili lagolago filifili, uili sprocket, uili taiala ma isi mea faapena. O loʻo iai pea le tupe na teuina.
e mafai ona fa'aaogaina meafaigaluega tungsten carbide.
O le UTP DUR 350 e matua lelei lava lona tete'e atu i le fa'apipi'iina ma le fa'asolosolo fa'atasi.
ma sina olo. E mafai ona fa'a'ele le u'amea fa'apipi'i i masini i meafaigaluega tungsten carbide.
Ma'a'a o le uelo mama e tusa ma le 370 HB
1 vaega i luga o u'amea ma le C = 0.5% pe tusa ma le 420 HB
Su'esu'ega masani i le %
C Si Mn Cr Fe
0.2 1.2 1.4 1.8 Paleni