Fa'amatalaga Pupuu:

O le ERCuSn-A Phos Bronze A o se apamemea-zinc bronze e tusa ma le 5% le tin ma e oo atu i le 0.35% le phosphorus e fa'aopoopo i ai e fai ma deoxidizer e fa'aaoga e fa'apipi'i ai le apamemea ma le apameme.


Fa'amatalaga o le oloa

Fa'ailoga o Oloa

O le RBCuZn-A Naval Bronze (RBCuZn-A) o se u'amea fa'atumu mo le fa'apipi'iina o le kopa-zinc o lo'o i ai ni nai apamemea e fa'aleleia atili ai le malosi ma le tete'e atu i le 'ele i totonu o le uelo. O se filifiliga lelei pe a le mana'omia ni uiga malolosi o le apamemea e itiiti le asu. E masani ona mana'omia se borax-boric acid flux pe a fa'apipi'iina i lenei oloa.

Vasega AWS: RBCuZn-A Fa'amaoniga: AWS A5.8/A5.8M:2011
U'amea fa'a'au'au: RBCuZn-A ASME SFA A5.8

 

Tulaga Fa'apipi'i: H, V Fa'asologa o le Fa'amalosi:
1330-1550⁰F

 

Malosiaga o le Fete'ena'iga, kpsi: 50
% o le fa'aloaloa, min: 30

 

Tulaga e liusuavai ai 1650⁰F Fa'amautu 1610⁰F Ma'a'a o Brinell 70-90

Kemisi Masani o Uaea e tusa ai ma le AWS A5.8 (o tau taʻitasi e maualuga)

Cu Zn Sn Pb Al Isi
57.0-61.0 Rem 0.25-1.00 0.05 0.01 0.50

 

Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua silia ma le 20 tausaga o matou galulue i le gaosiga o eletise uelo, u'amea uelo, ma mea e fa'aaogaina mo le uelo.

O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea e faia i le u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.

 

 

 

 


  • Muamua:
  • Sosoo ai: