Nikala Fa'a'au'auUaea Fa'apipi'iUaea TigERNiCrMo-4
| Tulaga Faatonuina |
| EN ISO 18274 – Ni 6276 – NiCr15Mo16Fe6W4 |
| AWS A5.14 – ER NiCrMo-4 |
Vaega ma Fa'aoga
E fa'aaogaina le ER-NiCrMo-4 mo le fa'apipi'iina o u'amea fa'atasi e tutusa o latou fa'asologa fa'akemikolo, e aofia ai mea eseese onikela-u'amea fa'avae, u'amea ma u'amea e le pala.
Ona o le maualuga o le molybdenum o lo'o iai, o lenei 'au'amea e tete'e atu ai i le māvaevae ma le 'ele, o le ta'ei o pitting ma le crevice correction.
E masani ona faʻaaogaina i paipa, vaʻa faʻamamafa, fale gaosi vailaʻau, fausaga suauʻu i fafo, fale gaosi kesi, gaosiga o le eletise ma siosiomaga o le gataifale ma isi mea faapena.
Meafaitino Faavae Masani
N10276, Numera W.: 2.4819, NiMo16Cr15W, U'amea Fa'afefiloi C4, U'amea Fa'afefiloi C276*
* O se lisi fa'a'āta'ita'i, ae le o se lisi atoa
| % o le Fa'atulagaga Fa'akemikolo | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | |
| sili ona maualuga | sili ona maualuga | sili ona maualuga | sili ona maualuga | sili ona maualuga | sili ona maualuga | |
| 0.05 | 0.80 | 0.70 | 0.030 | 0.010 | 0.75 | |
| Cu% | Ni% | Co% | Ti% | Al% | ||
| sili ona maualuga | 93.00 | sili ona maualuga | 2.00 | sili ona maualuga | ||
| 0.20 | minute | 1.00 | 3.50 | 1.00 | ||
| Meatotino Fa'amekanika | ||
| Malosiaga o le Fetaia'i | ≥690 MPa | |
| Malosiaga o le Tuuina Atu | - | |
| Fa'aloloa | - | |
| Malosiaga o le A'afiaga | - | |
E fa'atatau lava meatotino fa'ainisinia ma e ono fesuisuia'i e fa'atatau i le vevela, kasa puipuia, fa'atulagaga o le uelo ma isi mea.
Kasa Puipuia
EN ISO 14175 – TIG: I1 (Argon)
Tulaga o le Fa'avelaina
EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG
| Fa'amaumauga o le Afifiina | |||
| Lapo'a | Umi | Mamafa | |
| 1.60 milimita 2.40 milimita 3.20 milimita | 1000 milimita 1000 milimita 1000 milimita | 5 Kilokalama 5 Kilokalama 5 Kilokalama | |
Noataga: E ui ina ua faia taumafaiga talafeagai uma e faʻamautinoa ai le saʻo o faʻamatalaga o loʻo i totonu, o nei faʻamatalaga e mafai ona suia e aunoa ma se faʻaaliga ma e naʻo le taʻiala lautele e mafai ona manatu i ai.