Fa'amatalaga Pupuu:

E fa'aaogaina le ER-Ni1 mo le fa'avevela ma le ufiufiina o le Nickel 200 ma le Nickel 201 alloys.


Fa'amatalaga o le oloa

Fa'ailoga o Oloa

Nikala Fa'a'au'auUaea Fa'apipi'iUaea TigERNi-1

Tulaga Faatonuina
EN ISO 18274 – Ni 2061 – NiTi3
AWS A5.14 – ER Ni-1

 

Vaega ma Fa'aoga

E fa'aaogaina le ER-Ni1 mo le fa'avevela ma le ufiufiina o le Nickel 200 ma le Nickel 201 alloys.

E atoatoa mo le tu'ufa'atasia o le Monel alloys ma le copper-nikelau'amea fa'afefiloi i u'amea kaponi.

O lo'o iai i le Ni1 le titanium e lava e pulea ai le porosity o le u'amea fa'avevela i faiga fa'avevela.

E masani ona faʻaaogaina i pisinisi faʻagasologa o vailaʻau, gaosiga o alava faʻapitoa ma masini faʻagasologa o meaʻai ma isi mea faapena.

 

Meafaitino Faavae Masani

Nikel 200 ma le 201*
* O se lisi fa'a'āta'ita'i, ae le o se lisi atoa

 

% o le Fa'atulagaga Fa'akemikolo
C% Mn% Fe% P% S% Si%  
sili ona maualuga sili ona maualuga sili ona maualuga sili ona maualuga sili ona maualuga sili ona maualuga  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
sili ona maualuga 93.00 sili ona maualuga 2.00 sili ona maualuga    
0.20 minute 1.00 3.50 1.00    

 

Meatotino Fa'amekanika
Malosiaga o le Fetaia'i ≥410 MPa  
Malosiaga o le Tuuina Atu ≥200 MPa  
Fa'aloloa ≥30%  
Malosiaga o le A'afiaga ≥100 J  

E fa'atatau lava meatotino fa'ainisinia ma e ono fesuisuia'i e fa'atatau i le vevela, kasa puipuia, fa'atulagaga o le uelo ma isi mea.

 

Kasa Puipuia

EN ISO 14175 – TIG: I1 (Argon)

 

Tulaga o le Fa'avelaina

EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG

 

Fa'amaumauga o le Afifiina
Lapo'a Umi Mamafa  
1.60 milimita

2.40 milimita

1000 milimita

1000 milimita

5 Kilokalama

5 Kilokalama

 

 