O le ER4043 o se uaea alumini e fa'aaogaina lautele. O se tasi lea o uaea fa'apipi'i ma fa'apipi'i ua leva ma sili ona fa'aaogaina lautele. O lenei uaea alumini o lo'o i ai fa'aopoopoga silicon, lea e mafua ai ona fa'aleleia atili le sologa lelei o le vai fa'apipi'i ma e maua ai fo'i se uaea e le maaleale tele i le māvaevae. O lona susulu o le fa'apipi'iina e avea ai ma filifiliga lauiloa a le au fa'apipi'i. E mafai ona fa'aaoga le ER4043 e fa'apipi'i ai ituaiga eseese o alumini.
Fa'aoga Masani: uaea fa'atumu uelo; uaea u'amea fa'asusu ma afi
| Vasega AWS: ER4043 | Fa'amaoniga: AWS A5.10/ A5.10M:1999 |
| U'amea fa'a'ofu: ER4043 | AWS/ASME SFA A5.10 |
| Tulaga o le Fa'amauina: F, V, OH, H | Taimi nei: DCEP-GMAW AC-GTAW |
Meatotino Masani (e pei ona ueloina)
| Amioga: | 42% IACS (-12) |
| Malosiaga o le Fete'ena'iga, kpsi: | 29 |
| Lanu: | Lanu efuefu |
| Tulaga e liusuavai ai | 1170⁰F | Fa'amautu | 1065⁰F | Mafiafia | 0.097 pauna/kupita i totonu. |
Kemisi Masani o Uaea e tusa ai ma le AWS A5.10 (o tau taʻitasi e maualuga)
| Si | Fe | Cu | Mn | Mg | Zn | Ti | Isi | Al | ||||||
| 4.5-6.0 | 0.8 | 0.30 | 0.05 | 0.05 | 0.10 | 0.20 | 0.15 | Totoe | ||||||
| Fa'asologa Masani o le Fa'avelaina | ||||||||||||||
| Lapoa | Fa'agasologa | Volt | Fa'amālosi | Kasa | ||||||||||
| in | (mm) | |||||||||||||
| .030 | (.8) | GMAW | 15-24 | 60-175 | Argon (cfh) | |||||||||
| .035 | (.9) | GMAW | 15-27 | 70-185 | Argon (cfh) | |||||||||
| 3/64” | (1.2) | GMAW | 20-29 | 125-260 | Argon (cfh) | |||||||||
| 1/16” | (1.6) | GMAW | 24-30 | 170-300 | Argon (cfh) | |||||||||
| 3/32” | (2.4) | GMAW | 26-31 | 275-400 | Argon (cfh) | |||||||||
| Lapoa | Fa'agasologa | Volt | Fa'amālosi | Kasa | ||||||||||
| in | (mm) | |||||||||||||
| 1/16” | (1.6) | GTAW | 15 | 60-80 | Argon (cfh) | |||||||||
| 3/32” | (2.4) | GTAW | 15 | 125-160 | Argon (cfh) | |||||||||
| 1/8” | (3.2) | GTAW | 15 | 190-220 | Argon (cfh) | |||||||||
| 5/32” | (4.0) | GTAW | 15 | 200-300 | Argon (cfh) | |||||||||
| 3/16” | (4.8) | GTAW | 15-20 | 330-380 | Argon (cfh) | |||||||||
Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua silia ma le 20 tausaga o matou galulue i le gaosiga o eletise uelo, u'amea uelo, ma mea e fa'aaogaina mo le uelo.
O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea e faia i le u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.