O le E71T-GS o se u'amea kaponi, o se eletise e fa'aaogaina e aunoa ma se kesi puipui mai fafo. O lenei eletise ua fa'amoemoe mo le fa'apipi'iina o u'amea kaponi manifinifi, e amata mai le 3/16” i le 22 gauge.
Fa'aoga Masani: uelo e tasi le ala; o lenei oloa ua mamanuina e uelo lelei i luga o mea ua ueloina ma e mafai foi ona fa'aaogaina i nisi o mea ua ueloina i le alumini. E le mana'omia e le E71T-GS se puipuiga mai fafo ma e tatau ona ueloina i le DCEN (straight polarity).
| Vasega AWS: E71T-GS | Fa'amaoniga: AWS A5.20/A5.20M:2005 |
| U'amea fa'a'ofuofu: E71T-GS | AWS/ASME SFA A5.20 |
| Tulaga o le Fa'amauina: H, F, V, O | Taimi nei: DCEN Polarity sa'o |
| Malosiaga Fa'asaga i Luga o le Fa'alava, kpsi: | 86.4min (Mavaega o le u'amea autū) |
| Su'ega Pi'o Ta'ita'ia | Fa'ataunu'uina mana'oga o le AWS |
| Fa'asologa Masani o Uaea | |||||
| Lapoa | Fa'agasologa | Fa'amālosi | Volts | Saosaoa o le Fafagaina o Uaea | |
| in | (mm) | ||||
| .030″ | 0.8 | FCAW | 50 | 15 | 80 |
| FCAW | 100 | 16 | 225 | ||
| FCAW | 150 | 17 | 375 | ||
| FCAW | 175 | 17 | 445 | ||
| .035″ | 0.9 | FCAW | 75 | 15 | 70 |
| FCAW | 100 | 16 | 110 | ||
| FCAW | 150 | 17 | 180 | ||
| FCAW | 200 | 18 | 305 | ||
| .045″ | 1.2 | FCAW | 100 | 15 | 70 |
| FCAW | 150 | 16 | 120 | ||
| FCAW | 200 | 17 | 195 | ||
| FCAW | 225 | 17 | 245 | ||
| 1/6″ | 1.6 | FCAW | 150 | 17 | 60 |
| FCAW | 200 | 18 | 85 | ||
| FCAW | 250 | 18 | 135 | ||
| FCAW | 300 | 19 | 180 | ||
| 5/64” | .078 | FCAW | 200 | 19 | 60 |
| FCAW | 250 | 20 | 80 | ||
| FCAW | 300 | 21 | 115 | ||
| FCAW | 325 | 120 | 6.6 | ||
Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua matou galulue i le gaosiga o eletise uelo,u'amea fa'apipi'i, ma mea fa'aaogā mo le ueloina mo le silia ma le 20 tausaga.
O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.