Uaea U'amea e le gaoia AWS ER308L, La'au U'amea MIG ma TIG, La'au Fa'atumu

Fa'amatalaga Pupuu:

E maualuga le lelei o le fa'apipi'iina o le uaea u'amea e le gaoia, ma e lelei fo'i le fa'atinoga fa'apitoa o le u'amea i so'o se tulaga. E fa'aaogaina lautele i pisinisi: fausaga o fale, ta'avale, inisinia o alalaupapa, masini eliina ai minerale, ala u'amea, paipa suau'u, masini e tauaveina le mamafa o le kesi, masini eletise, ma isi mea fa'apena.


Fa'amatalaga o le oloa

Fa'ailoga o Oloa

Fa'avasegaga AWS: AWS 5.9

FA'AMATALAGA:

O le uaea u'amea e le gaoia e maualuga lona lelei i le ufiufi, ma e lelei fo'i lona fa'atinoga fa'apitoa i le u'amea i so'o se tulaga. E fa'aaogaina lautele i pisinisi: fausaga o fale, ta'avale, inisinia o alalaupapa, masini eliina ai minerale, alalaupapa, paipa suau'u, masini e tauaveina le mamafa o le kesi, masini eletise, ma isi mea fa'apena.

FA'ATA'ITA'IGA NUMERA & TELE:

1. Sapalai oloa a le falegaosimea tautua OEM.

2. Fa'ata'ita'iga: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi ma isi.

3. Tele o le uaea MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4. Tele o le uaea TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.

FA'ATOMUAGA:

Matou te tuʻuina atu ituaiga eseese o uaea uʻamea e le gaoia ai mea, e aofia ai uaea uʻamea malosi Mig, uaea uʻamea Tig rod ma uaea uʻamea submerged-arc, o mea uma ia e maualuga le tulaga lelei ma e faʻatau atu i le lalolagi atoa.

Se'i vagana ai le 308 ma le 309, matou te ofoina atu fo'i le 304, 321, 347, 316L, 310, 2209, ma le 201. Fa'apea fo'i ma fa'amatalaga fa'apitoa e pei o le 318L, 904L, 2594, NiCrMo-3, Ni1.

AFIFIINA:

Afifiina o uaea uelo Mig (afifi o spool ma le drum)

Lapoa: 0.8 - 2.0mm

Afifi: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/drum, 200 kg/drum

Uaea uelo o le Tig rod ua afifiina (paipa palasitika)

Lapoa: 1.0 - 5.0mm

Afifi: 5 kg/afifi

Uaea uelo fa'asolo i lalo o le vai

Lapoa: 2.5 - 5.0mm

Afifi: 20kg/afifi, 25 kg/afifi

E talia le afifiina e le faaituau ma le OEM!

FA'AVAEGA FA'AKEMIKOLO O LE UAEA U'AMEA E LEAI SE PISINISI:

Fa'ata'ita'iga Nu.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

UIGA FA'AMEKANIKA O LE UAEA FA'AVEVELI:

Fa'ata'ita'iga Nu.

Malosiaga o le tensile Rm(Mpa)

Malosiaga o le gaosiga Rel po'o le Rp0.2 (Mpa)

Fa'aloloa

(%)

Fa'ata'ita'iga Nu.

Malosiaga o le tensile Rm(Mpa)

Malosiaga o le gaosiga Rel po'o le Rp0.2 (Mpa)

Fa'aloloa

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

O le tuufaatasiga o uaea u'amea e le gaoia TIG ma MIG

YB5092-2005

AWS

% o le Fa'atulagaga Fa'akemikolo

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Cu 1.80

H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Cu;3 Nb;0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua silia ma le 20 tausaga o matou galulue i le gaosiga o eletise uelo, u'amea uelo, ma mea e fa'aaogaina mo le uelo.

O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea e faia i le u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.

 

Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua silia ma le 20 tausaga o matou galulue i le gaosiga o eletise uelo, u'amea uelo, ma mea e fa'aaogaina mo le uelo.

O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea e faia i le u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.