Fa'avasegaga AWS: AWS 5.9
FA'AMATALAGA:
O le uaea u'amea e le gaoia e maualuga lona lelei i le ufiufi, ma e lelei fo'i lona fa'atinoga fa'apitoa i le u'amea i so'o se tulaga. E fa'aaogaina lautele i pisinisi: fausaga o fale, ta'avale, inisinia o alalaupapa, masini eliina ai minerale, alalaupapa, paipa suau'u, masini e tauaveina le mamafa o le kesi, masini eletise, ma isi mea fa'apena.
FA'ATA'ITA'IGA NUMERA & TELE:
1. Sapalai oloa a le falegaosimea tautua OEM.
2. Fa'ata'ita'iga: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi ma isi.
3. Tele o le uaea MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Tele o le uaea TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.
FA'ATOMUAGA:
Matou te tuʻuina atu ituaiga eseese o uaea uʻamea e le gaoia ai mea, e aofia ai uaea uʻamea malosi Mig, uaea uʻamea Tig rod ma uaea uʻamea submerged-arc, o mea uma ia e maualuga le tulaga lelei ma e faʻatau atu i le lalolagi atoa.
Se'i vagana ai le 308 ma le 309, matou te ofoina atu fo'i le 304, 321, 347, 316L, 310, 2209, ma le 201. Fa'apea fo'i ma fa'amatalaga fa'apitoa e pei o le 318L, 904L, 2594, NiCrMo-3, Ni1.
AFIFIINA:
Afifiina o uaea uelo Mig (afifi o spool ma le drum)
Lapoa: 0.8 - 2.0mm
Afifi: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/drum, 200 kg/drum
Uaea uelo o le Tig rod ua afifiina (paipa palasitika)
Lapoa: 1.0 - 5.0mm
Afifi: 5 kg/afifi
Uaea uelo fa'asolo i lalo o le vai
Lapoa: 2.5 - 5.0mm
Afifi: 20kg/afifi, 25 kg/afifi
E talia le afifiina e le faaituau ma le OEM!
FA'AVAEGA FA'AKEMIKOLO O LE UAEA U'AMEA E LEAI SE PISINISI:
| Fa'ata'ita'iga Nu. | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Fa'ata'ita'iga Nu. | Malosiaga o le tensile Rm(Mpa) | Malosiaga o le gaosiga Rel po'o le Rp0.2 (Mpa) | Fa'aloloa (%) | Fa'ata'ita'iga Nu. | Malosiaga o le tensile Rm(Mpa) | Malosiaga o le gaosiga Rel po'o le Rp0.2 (Mpa) | Fa'aloloa (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| O le tuufaatasiga o uaea u'amea e le gaoia TIG ma MIG | ||||||||||
| YB5092-2005 | AWS | % o le Fa'atulagaga Fa'akemikolo | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu;3 Nb;0.28 | |
| H08Cr26Ni5Mo2 | ER453s | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N;0.20 V;0.18 |
Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua silia ma le 20 tausaga o matou galulue i le gaosiga o eletise uelo, u'amea uelo, ma mea e fa'aaogaina mo le uelo.
O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea e faia i le u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.
Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua silia ma le 20 tausaga o matou galulue i le gaosiga o eletise uelo, u'amea uelo, ma mea e fa'aaogaina mo le uelo.
O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea e faia i le u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.