AWS: Uaea E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4 ua fa'apipi'i i le Flux-cored (FCAW-G)ua mamanuina mo galuega malolosi, maualalo le u'amea e fa'aaogaina ai le 100% kasa puipuia o le CO2.
Fa'aaliga
E mafai ona gaosia ni fa'aputuga uelo ma le malosi e sili atu i le 88 – 123 J (65 – 91 ft·lbf) i le -40°C (-40°F)
Fuafuaina mo le fa'avevela ma le 100% CO2 protective gas
Fa'atinoga sili ona lelei o le arc ma le foliga vaaia o beads
Ua ausia mana'oga o le AWS D1.8 mo le fa'amagaloina o le fa'aleagaina o le fanua fa'alenatura
afifiina o le taga pepa alumini
| FETU'UNA'I | FA'AMATALAGA | FA'AVAEGA |
| AWS | AWS A5.29 | E81T1-Ni1C-JH4 |
| AWS | AWS A5.36 | E81T1-C1 A4-Ni1-H4 |
| ABS | ABS- Vaega 2 | 4YQ460SA H5 |
| CWB | CSA W48 | E551T1-C1A4-Ni1-H4 (E551T1-Ni1C-JH4) |
| DNV-GL | DNV-2.9 IV | Y46MS H5 |
| LR | LR – Mataupu 11 | 4Y46S H5 |
FA'ATULAGA O LE TEUINA O TUPE
| Fa'avasegaga | Kasa Puipuia | Polarity | %B | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %SI | %V | Haidrone e Faasalalauina mL/100g U'amea Fa'apipi'i |
| E81T1-Ni1C-JH4 | 100% CO2 | DC+ | 0.12 maualuga | 0.15 maualuga | 1.5 maualuga | 0.35 maualuga | 0.8-1.1 | 0.03 maualuga | 0.03 maualuga | 0.8 maualuga | 0.05 maualuga | 4.0 maualuga | |
| E81T1-C1A4-Ni1-H4 | 100% CO2 | DC+ | 0.12 maualuga | 0.15 maualuga | 1.75 maualuga | 0.35 maualuga | 0.8-1.1 | 0.03 maualuga | 0.03 maualuga | 0.8 maualuga | 0.05 maualuga | 4 maualuga. | |
| Iʻuga Masani, E pei ona faʻapipiʻiina | 100% CO2 | DC+ | 0.0050-0.006 | 0.04-0.05 | 0.04-0.06 | 1.12-1.42 | 0.01 | 0.81-1 | 0.012 maualuga | 0.01 maualuga | 0.24-0.35 | 0.02- 0.03 | 1.7-3.2 |
FA'AMATALAGA
Mo le fuafuaina o le ESO, to'ese le 1/4 inisi (6.0 mm) mai le CTWD.
FA'AMATALAGA 1: O fa'amatalaga fa'aopoopo o su'ega fa'ale-seismic o le FEMA ma le AWS D1.8 e mafai ona maua i luga o lenei oloa i le www.lincolnelectric.com.
FA'AMATALAGA 2: O lenei oloa o lo'o i ai elemene micro-alloying. O fa'amatalaga fa'aopoopo e maua pe a talosagaina.
Na faavaeina le Wenzhou Tianyu Electronic Co., Ltd. i le 2000. Ua matou galulue i le gaosiga o eletise uelo,u'amea fa'apipi'i, ma mea fa'aaogā mo le ueloina mo le silia ma le 20 tausaga.
O a matou oloa autū e aofia ai eletise u'amea e le gaoia, eletise u'amea kaponi, eletise u'amea e maualalo le u'amea, eletise u'amea e fa'apipi'i i luga, eletise u'amea e faia i le nickel ma le cobalt alloy, uaea u'amea e faia i le u'amea vaivai ma le u'amea maualalo le u'amea, uaea u'amea e le gaoia, uaea u'amea e puipuia i le kesi, uaea u'amea alumini, uaea u'amea e fa'apipi'i i le arc i lalo, uaea u'amea, uaea u'amea nickel ma le cobalt alloy, uaea u'amea apameme, uaea u'amea TIG ma le MIG, eletise tungsten, eletise e fa'apipi'i ai le kaponi, ma isi mea fa'aopoopo ma mea e fa'aaogaina mo le u'amea.