AWS A5.18 ER70S-6 Uaea U'amea Fa'apipi'i Uamea mo le Fa'apipi'iina o le 'Arc Welding' e Puipuia e le Kasa, Uaea Malolo

Fa'amatalaga Pupuu:

O le ER70S6 o se uaea u'amea vaivai e maualuga atu le manganese ma le silicon nai lo isi vasega masani o uaea MIG e gaosia ai ni u'amea lelei pe a fa'aaogaina i u'amea palapala, ga'o, pe 'elea.


Fa'amatalaga o le oloa

Fa'ailoga o Oloa

O le ER70S6 o se uaea u'amea vaivai e maualuga atu le manganese ma le silicon nai lo isi vasega masani o uaea MIG e gaosia ai ni u'amea lelei pe a fa'aaogaina i u'amea palapala, ga'o, po'o le 'ele'elea. O le maualuga o le silicon e fa'ateleina ai le sologa lelei o le u'amea, ma fa'atupuina ai se foliga lamolemole ma i'u ai i le la'ititi o le oloina pe a uma ona u'amea. O lenei uaea ua mamanuina e tu'uina atu ai ni u'amea e leai ni porosity, lelei o le x-ray i le malosi sili ona maualuga (e pei ona u'uina) o uaea u'amea carbon masani uma.

Fa'aoga Masani: fa'aoga lautele i faleoloa e le lelei le fetaui pe 'elea ma suāu'u; u'amea fa'apala pe u'amea fa'aola; galuega fa'atino i le fale; laupepa u'amea; tane; galuega faufale

Vasega AWS: ER70S6

Fa'amaoniga: AWS A5.18/A5.18M:2005

U'amea fa'a'amea: ER70S6

ASME SFA A5.18

Tulaga Fa'apipi'i: F, V, OH, H

Taimi nei: DCEP

Malosiaga o le Fete'ena'iga, kpsi:

70

Malosiaga o le Fua, kpsi:

58

Fa'aloloa i le 2”%:

22

Kemisi Masani o Uaea e tusa ai ma le AWS A5.18 (o tau taʻitasi e maualuga)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1.85

0.80-1.15

0.025

0.035

0.15

0.15

0.15

0.03

0.50

Fa'asologa Masani o le Fa'avelaina

Lapoa

Fa'agasologa

Volt

Saosaoa o le Malaga

Fa'amālosi

Kasa Puipuia

in

(mm)

(ipm)

.035

(0.9)

GMAW

23-26

11-22

160-300

Fa'aliliuina o le Suāvai 98% Argon+2% Okesene

.045

(1.2)

GMAW

23-29

12-21

170-375

Fa'aliliuina o le Suāvai 98% Argon+2% Okesene

1/16

(1.6)

GMAW

25-31

9-19

275-475

Fa'aliliuina o le Suāvai 98% Argon+2% Okesene

.023

GMAW

14-19

10-15

30-85

Fesiitaiga o le Taamilosaga Pupuu 98% Argon+2% Okesene

.030

(0.8)

GMAW

15-20

12-24

40-130

Fesiitaiga o le Taamilosaga Pupuu 98% Argon+2% Okesene

.035

(0.9)

GMAW

16-25

11-40

60-235

Fesiitaiga o le Taamilosaga Pupuu 98% Argon+2% Okesene

.045

(1.14)

GMAW

18-23

12-22

90-290

Fesiitaiga o le Taamilosaga Pupuu 98% Argon+2% Okesene

.035

(0.9)

GTAW

12-15

Leai se totogi

60-100

100% Argon

.045

(1.14)

GTAW

13-16

Leai se totogi

70-120

100% Argon

1/16

(1.6)

GTAW

12

Leai se totogi

100-160

100% Argon

1/16- 3/32

(1.6)-(2.4)

GTAW

12

Leai se totogi

120-250

100% Argon

1/8

(3.2)

GTAW

12

Leai se totogi

150-300

100% Argon


  • Muamua: